C | Si | Mn | P | S | Cr | Mo | W | V | Co | Ni |
---|---|---|---|---|---|---|---|---|---|---|
0,73-0,83 | Max 0,45 | - | Max 0,030 | Max 0,030 | 3,80- 4,50 | - | 17,12-18,70 | 1,00-1,20 | - | - |
Hardness after | Tempering ºC | Symbol | Value |
Soft annealinh | - | HB | ≤269 |
Quenching with 1260 ºC in oil | - | HRC | 63 |
Quenching with 1260 ºC in oil and tempering (cooling during quenching can be performed gradually in the salt bath at the temperature of around 550 ºC and then cooled in the air) | 350 | HRC | 62 |
400 | HRC | 62 | |
450 | HRC | 63.5 | |
500 | HRC | 64.5 | |
550 | HRC | 65 | |
600 | HRC | 63 | |
650 | HRC | 59 | |
700 | HRC | 48 |
Property | Unit | Value |
Density, ρ | g*cm-3 | 8.61 |
Technological treatment processes | Possible application | Temperature, °C | ||
Hot forming | Forging | + | 1150-900 | |
Rolling | + | 1150-900 | ||
Heat treatment | Soft annealing | + | 800-900 | |
Stress relieving | + | 600-700 | ||
Quenching | Heating I | + | ~550 | |
Heating II | + | 850 | ||
Austenitising | + | 1230-1270 | ||
Tempering | + | 550-570 | ||
Surface treatment | Nitriding | + | 510-530 | |
Coat application | + | PVD |
ISO | CEN | Russia | |||
HS18-0-1 | ISO 4957:2004 | HS18-0-1 | ISO 4957:2004 | R18 | GOST 19265-73 |
US | Japan | China | |||
T1 | ASTM A 600-92 | SKH 2 | JIS G 4403-1983 | W18Cr4V | GB 9943-88 |