Still deciding? Get samples of $ !
Request Sample
|
| Customization: | Available |
|---|---|
| Type: | Round |
| Standard: | AISI, ASTM, DIN, JIS, GB, BS |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency








| C | Si | Mn | P | S | Cr | Mo | W | V | Co | Ni |
|---|---|---|---|---|---|---|---|---|---|---|
| 0,5-0,6 | 0,10-0,40 | 0,60 - 0,90 | MAX 0,03 | MAX 0,03 | 0,80-1,20 | 0,35-0,55 | - | 0,05-0,15 | - | 1,50-1,80 |
| Hardness after | Tempering ºC | Symbol | Value |
| Soft annealing | - | HB | ≤248 |
| Quenching with 850 ºC in oil | - | HRC | 60 |
| Quenching with 850 ºC in oil and tempering
(cooling during quenching can be in the forced air or polymer) |
500 | HRC | 42 |
| 350 | HRC | 52.5 | |
| 400 | HRC | 51 | |
| 450 | HRC | 49 | |
| 500 | HRC | 47 | |
| 550 | HRC | 44.5 | |
| 600 | HRC | 42 |
| Property | Unit | Value |
| Density, ρ | g*cm-3 | 7.85 |
| Linear expansivity, α20-100ºC) | K-1 | 12*10-6 |
| Specific thermal conductivity, λ20ºC) | W*m-1*K-1 | 34 |
| Technological treatment processes | Possible application | Temperature, °C | ||
| Hot forming | Forging | + | 1100-850 | |
| Rolling | + | 1100-850 | ||
| Treatment | Heat treatment | Quenching | + | 840-890 |
| Tempering | + | 500-600 | ||
| Precipitation strengthening | Supersaturation | - | - | |
| Ageing | - | - | ||
| Annealing | Soft annealing | + | 650-680 | |
| Stress relieving | + | 600-650 | ||
| Thermochemical treatment | Nitriding | - | - | |
| Other | - | - | ||
| ISO | CEN | Russia | |||
| 55NiCrMoV7 | ISO 4957:2004 | 55NiCrMoV7 | ISO 4957:2004 | ~5HNM | GOST 5950-73 |
| US | Japan | China | |||
| ~L6 | ASTM A 681-91 | ~SKT 4 | JIS G 4404-1983 | ~5CrNiMo | GB 1299-85 |