Customization: | Available |
---|---|
Type: | Round |
Standard: | AISI, ASTM, DIN, JIS, GB, BS |
Still deciding? Get samples of US$ 1000/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
About Product
Country | USA | German | Japan | British |
Standard | ASTM A681 | DIN EN ISO 4957 | JIS G4404 | BS 4659 |
Grades | H11/T20811 | 1.2343/X37CrMoV5-1 | SKD6 | BH11 |
ASTM A681 | C | Mn | P | S | Si | Cr | V | W | Mo | ||||||
H11/T20811 | 0.35 | 0.45 | 0.20 | 0.60 | 0.03 | 0.03 | 0.80 | 1.25 | 4.75 | 5.50 | 0.30 | 0.60 | … | 1.10 | 1.60 |
DIN ISO 4957 | C | Mn | P | S | Si | Cr | V | W | Mo | ||||||
1.2343/X37CrMoV5-1 | 0.33 | 0.41 | 0.25 | 0.5 | … | … | 0.80 | 1.20 | 4.8 | 5.5 | 0.3 | 0.5 | … | 1.10 | 1.50 |
JIS G4404 | C | Mn | P | S | Si | Cr | V | W | Mo | ||||||
SKD6 | 0.32 | 0.42 | … | 0.50 | 0.03 | 0.03 | 0.80 | 1.20 | 4.50 | 5.50 | 0.30 | 0.50 | … | 1.00 | 1.50 |
BS 4659 | C | Mn | P | S | Si | Cr | V | W | Mo | ||||||
BH11 | 0.32 | 0.40 | … | 0.40 | 0.35 | 0.35 | 0.85 | 1.15 | 4.75 | 5.25 | 0.30 | 0.50 | … | 1.25 | 1.75 |
Properties | Metric | Imperial |
Density | 7.81 g/cm3 | 0.282 lb/in3 |
Melting point | 1427°C | 2600°F |
Properties | Metric | Imperial |
Hardness, Rockwell C (air cooled from 982°C, 45 mins) | 52.5 | 52.5 |
Hardness, Rockwell C (air cooled from 1010°C, 45 mins) | 56 | 56 |
Hardness, Rockwell C (air cooled from 1038°C, 45 mins) | 57 | 57 |
Modulus of elasticity | 207 GPa | 30000 ksi |
Modulus of elasticity (@538°C/1000°F) | 159 GPa | 23000 ksi |
Modulus of elasticity (@204°C/400°F) | 190 GPa | 27500 ksi |
Charpy impact (V-notch; air cooled from 1010°C;535°C temper temperature) | 13.6 J | 10.0 ft-lb |
Charpy impact (V-notch; air cooled from 1010°C;650°C temper temperature) | 27.1 J | 20.0 ft-lb |
Charpy impact (V-notch; air cooled from 1010°C;370°C temper temperature) | 33.9 J | 25.0 ft-lb |
Machinability (1% carbon steel) | 75.0 - 80.0% | 75.0 - 80.0% |
Poisson's ratio | 0.27-0.30 | 0.27-0.30 |
Properties | Metric | Imperial |
Thermal expansion (@20-100ºC/68-212ºF) | 11.9 x 10-6/ºC | 6.63 µin/in°F |
Thermal conductivity (@100ºC/212ºF) | 42.2 W/mK | 292.9 in/hr.ft².°F |