Customization: | Available |
---|---|
Type: | Carbon Steel Bar |
Standard: | AISI, ASTM, DIN, JIS, GB, BS |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
C | Si | Mn | P | S | Cr | Mo | W | V | Co | Ni |
---|---|---|---|---|---|---|---|---|---|---|
0,33-0,45 | ≤1,00 | ≤1,50 | Max 0,030 | Max 0,030 | 15,50-17,50 | 0,80-1,30 | - | - | - | ≤1,00 |
Hardness after | Tempering ºC | Symbol | Value |
Soft annealing | - | HB | ≤250 |
Toughening | HB | 300 | |
Quenching with 1010 ºC in oil | - | HRC | 49 |
Quenching with 1010 ºC in oil and tempering
(cooling during quenching can also be gradual in the salt bath at 500-550 ºC and then in the air) |
200 | HRC | 47 |
300 | HRC | 46 | |
400 | HRC | 36.5 | |
450 | HRC | 37 | |
500 | HRC | 43 | |
550 | HRC | 38 | |
600 | HRC | 32.5 |
Property | Unit | Value |
Density, ρ | g*cm-3 | 7.6 |
Thermal expansion, α20-100ºC) | K-1 | 10.4*10-6 |
Thermal conductivity, λ20ºC) | W*m-1*K-1 | 26 |
Technological treatment processes | Possible application | Temperature, °C | ||
Hot forming | Forging | + | 1100-750 | |
Rolling | + | 1100-750 | ||
Treatment | Heat treatment | Quenching | + | 1000-1040 |
Tempering | + | 550-650 | ||
Precipitation strengthening | Supersaturation | - | - | |
Ageing | - | - | ||
Annealing | Soft annealing | + | 780-820 | |
Stress relieving | + | 600-700 | ||
Thermochemical treatment | Nitriding | + | 470-550 | |
Other | - | - |
ISO | CEN | Russia | |||
X38CrMo16 | ISO 4957:2004 | X38CrMo16 | ISO 4957:2004 | - | - |
US | Japan | China | |||
- | - | - | - | - | - |