Customization: | Available |
---|---|
Type: | Flat |
Standard: | AISI, ASTM, DIN, JIS, GB, BS |
Still deciding? Get samples of US$ 2000/Ton
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
C | Si | Mn | P | S | Cr | Mo | W | V | Co | Ni |
---|---|---|---|---|---|---|---|---|---|---|
0,36-0,42 | Max 1,00 | Max 1,00 | Max 0,030 | Max 0,030 | 12,50-14,50 | - | - | - | - | - |
Hardness after | Tempering ºC | Symbol | Value |
Soft annealing | - | HB | ≤241 |
Toughening | HB | 300 | |
Quenching with 1010 ºC in oil | - | HRC | 54 |
Quenching with 1010 ºC in oil and tempering
(cooling during quenching can also be performed either in the air or gradually in the salt bath at 500-550 ºC and then cooled in the air) |
180 | HRC | ≥52 |
200 | HRC | 53 | |
250 | HRC | 52.5 | |
450 | HRC | 54 | |
500 | HRC | 52.5 | |
550 | HRC | 49.5 | |
600 | HRC | 46 |
Property | Unit | Value |
Density, ρ | g*cm-3 | 7.60 |
Thermal expansion, α20-100ºC) | K-1 | 10.6*10-6 |
Thermal conductivity, λ20ºC) | W*m-1*K-1 | 29 |
Technological treatment processes | Possible application | Temperature, °C | ||
Hot forming | Forging | + | 1100-800 | |
Rolling | + | 1100-800 | ||
Treatment | Heat treatment | Quenching | + | 1000-1050 |
Tempering | + | 150-300
400-600 |
||
Precipitation strengthening | Supersaturation | - | - | |
Ageing | - | - | ||
Annealing | Soft annealing | + | 750-800 | |
Stress relieving | + | 600-700 | ||
Thermochemical treatment | Nitriding | + | 470-520 | |
Other | - | - |
ISO | CEN | Russia | |||
X40Cr14 | ISO 4957:2004 | X40Cr14 | ISO 4957:2004 | - | - |
US | Japan | China | |||
- | - | - | - | - | - |