C | Si | Mn | P | S | Cr | Mo | W | V | Co | Ni |
---|---|---|---|---|---|---|---|---|---|---|
0,18-0,24 | 0,15-0,35 | 1,10-1,40 | Max 0,030 | Max 0,030 | 1,00 - 1,30 | - | - | - | - | - |
Hardness after | Tempering ºC | Symbol | Value |
Soft annealing | - | HB | ≤217 |
Quenching1) with 820 ºC in water | - | HRC | 62 |
Quenching1) with 820 ºC in water and tempering
1) after carburising |
180 | HRC | ≥60 |
200 | HRC | 60 | |
250 | HRC | 58.5 | |
300 | HRC | 57 | |
350 | HRC | 55 | |
400 | HRC | 53.5 | |
450 | HRC | 52 | |
500 | HRC | 50.5 |
Property | Unit | Value |
Density. ρ | g*cm-3 | 7.85 |
Thermal expansion. α20-100ºC) | K-1 | 11.9*10-6 |
Thermal conductivity. λ20ºC) | W*m-1*K-1 | 52 |
Technological treatment processes | Possible application | Temperature. °C | ||
Hot forming | Forging | + | 1100-850 | |
Rolling | + | 1100-850 | ||
Treatment | Heat treatment | Quenching | + | 810-830 |
Tempering | + | 170-190 | ||
Precipitation strengthening | Supersaturation | - | - | |
Ageing | - | - | ||
Annealing | Softening | + | 660-700 | |
Stress relieving | + | 600-680 | ||
Thermochemical treatment | Nitriding | - | 880-950 | |
Other | - | 880-920 |
ISO | CEN | Russia | |||
21MnCr5 | ISO 4957:1999 | 21MnCr5 | EN ISO 4957:1999 | - | - |
US | Japan | China | |||
- | - | - | - | - | - |