C | Si | Mn | P | S | Cr | Mo | W | V | Co | Ni |
---|---|---|---|---|---|---|---|---|---|---|
0,55-0,65 | 0,70-1,00 | 0,15-0,45 | Max 0,030 | Max 0,030 | 0,90-1,20 | - | 1,70-2,20 | 0,10-0,20 | - | - |
Hardness after | Tempering ºC | Symbol | Value |
Soft annealing | - | HB | ≤229 |
Quenching with 910 ºC in oil | - | HRC | 62.5 |
Quenching with 910 ºC in oil and tempering | 180 | HRC | ≥58 |
200 | HRC | 60 | |
225 | HRC | 59.5 | |
250 | HRC | 59 | |
300 | HRC | 57.5 | |
350 | HRC | 55.5 | |
400 | HRC | 53.5 | |
450 | HRC | 51 |
Property | Unit | Value |
Density, ρ | g*cm-3 | 7.95 |
Thermal expansion, α20-100ºC) | K-1 | 12.4*10-6 |
Thermal conductivity, λ55ºC) | W*m-1*K-1 | 34.2 |
Technological treatment processes | Possible application | Temperature, °C | ||
Hot forming | Forging | + | 1050-850 | |
Rolling | + | 1050-850 | ||
Treatment | Heat treatment | Quenching | + | 900-920 |
Tempering | + | 170-190 | ||
Precipitation strengthening | Supersaturation | - | - | |
Ageing | - | - | ||
Annealing | Soft annealing | + | 710-740 | |
Stress relieving | + | 600-700 | ||
Thermochemical treatment | Nitriding | - | - | |
Other | - | - |
ISO | CEN | Russia | |||
60WCrV8 | ISO 4957:2004 | 60WCrV8 | ISO 4957:2004 | ~6HW2SF | GOST 5950-73 |
US | Japan | China | |||
~S1 | ASTM A 681-91 | - | - | ~6CrW2Si | GB 1299-85 |